SiO₂
DCI Tailor Spatial Atlas
Community Verified XRF/pXRF & Geological Reference Assays
Public Atlas Assays
62
Community Verified (2.5× Prior)
0
USGS / Academic Surveys
62
Mapped Lithologies
15
Regional Geochemical Map
Community XRF / pXRF USGS / Academic Survey

Marl

USGS DS-801 XRD marl 36.4072, -105.5731
4-Acid ICP + Rietveld QXRD ID: DS801-NM-012-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
56.38%
Al2O3
12.55%
Fe₂O₃(T)
3.67%
CaO
10.04%
MgO
2.49%
K2O
2.51%
Na2O
1.63%
LOI
9.92%

Alluvial Clay

USGS DS-801 XRD alluvial clay 40.6187, -80.5773
4-Acid ICP + Rietveld QXRD ID: DS801-OH-011-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
63.72%
Al2O3
20.16%
Fe₂O₃(T)
4.57%
CaO
0.66%
MgO
1.21%
K2O
2.78%
Na2O
0.42%
LOI
5.21%

Kaolin Clay

USGS DS-801 XRD kaolin clay 36.7417, -88.6367
4-Acid ICP + Rietveld QXRD ID: DS801-KY-010-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
61.06%
Al2O3
24.94%
Fe₂O₃(T)
2.04%
CaO
0.30%
MgO
0.52%
K2O
1.36%
Na2O
0.24%
LOI
8.00%

Glacial Clay

USGS DS-801 XRD glacial clay 42.0347, -93.6200
4-Acid ICP + Rietveld QXRD ID: DS801-IA-009-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
61.91%
Al2O3
11.90%
Fe₂O₃(T)
3.98%
CaO
7.11%
MgO
2.79%
K2O
1.98%
Na2O
1.29%
LOI
8.29%

Kaolin Clay

USGS DS-801 XRD kaolin clay 32.9815, -82.8101
4-Acid ICP + Rietveld QXRD ID: DS801-GA-008-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
56.52%
Al2O3
29.14%
Fe₂O₃(T)
1.91%
CaO
0.17%
MgO
0.26%
K2O
0.62%
Na2O
0.12%
LOI
9.63%

Alluvial Clay

USGS DS-801 XRD alluvial clay 45.7090, -121.5290
4-Acid ICP + Rietveld QXRD ID: DS801-OR-007-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
56.24%
Al2O3
16.74%
Fe₂O₃(T)
9.57%
CaO
4.25%
MgO
3.11%
K2O
1.07%
Na2O
2.49%
LOI
4.22%

Alluvial Clay

USGS DS-801 XRD alluvial clay 44.9429, -123.0351
4-Acid ICP + Rietveld QXRD ID: DS801-OR-006-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
63.10%
Al2O3
16.98%
Fe₂O₃(T)
6.66%
CaO
2.22%
MgO
1.88%
K2O
1.83%
Na2O
2.01%
LOI
4.02%

Loess

USGS DS-801 XRD loess 46.8450, -117.3620
4-Acid ICP + Rietveld QXRD ID: DS801-WA-005-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
68.15%
Al2O3
13.72%
Fe₂O₃(T)
4.92%
CaO
2.94%
MgO
1.82%
K2O
2.36%
Na2O
2.22%
LOI
2.75%

Kaolin Clay

USGS DS-801 XRD kaolin clay 47.5620, -117.1050
4-Acid ICP + Rietveld QXRD ID: DS801-WA-004-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
60.28%
Al2O3
25.32%
Fe₂O₃(T)
2.29%
CaO
0.57%
MgO
0.61%
K2O
2.87%
Na2O
0.89%
LOI
6.21%

Glacial Clay

USGS DS-801 XRD glacial clay 47.6120, -122.5340
4-Acid ICP + Rietveld QXRD ID: DS801-WA-003-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
60.92%
Al2O3
16.66%
Fe₂O₃(T)
6.44%
CaO
3.25%
MgO
2.65%
K2O
2.16%
Na2O
2.38%
LOI
4.42%

Alluvial Clay

USGS DS-801 XRD alluvial clay 47.1910, -122.2980
4-Acid ICP + Rietveld QXRD ID: DS801-WA-002-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
64.66%
Al2O3
15.98%
Fe₂O₃(T)
5.74%
CaO
2.64%
MgO
2.00%
K2O
2.03%
Na2O
2.45%
LOI
3.48%

Glacial Clay

USGS DS-801 XRD glacial clay 47.2580, -122.4520
4-Acid ICP + Rietveld QXRD ID: DS801-WA-001-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
63.90%
Al2O3
15.59%
Fe₂O₃(T)
6.07%
CaO
2.94%
MgO
2.30%
K2O
1.91%
Na2O
2.57%
LOI
3.67%